Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.9 GPa | 1730 ksi | d.a.m.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® BKV 40 H2.0 901510 Nylon 6, Glass Fiber Reinforced PA 6, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 11.9 GPa | 1730 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® AE-8930 Polyphthalamide (PPA), 30% Glass Fiber Amodel® AE-8930 is a 30% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Glycol Resistant; Good Chemical Resistance; Good Creep .. |
|||
Tensile Modulus | 11.9 GPa | 1730 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® DW-1130 Polyphthalamide (PPA), 30% Glass Fiber Amodel® DW-1130 is a 30% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient o.. |
|||
Tensile Modulus | 11.9 GPa | 1730 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® SHF436HR PBT PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant. |
|||
Tensile Modulus | 11.9 GPa | 1730 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® SHF436HR PBT (Asia Pacific) PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant. |
|||
Tensile Modulus | 11.9 GPa | 1730 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® SHF436HR PBT (Europe-Africa-Middle East) PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant. |
|||
Tensile Modulus | 11.9 GPa | 1730 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF008ESY PA 66 LNP THERMOCOMP* RF008ESY is a compound based on Nylon 66 resin containing 40% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Tensile Modulus | 11.9 GPa | 1730 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RV007SX9 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV007SX9 is a compound based on PA 66 resin containing Long Glass Fiber. |
|||
Tensile Modulus | 11.9 GPa | 1730 ksi | |
Radici Radilon® A RV350 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Tensile Modulus | 11.9 GPa | 1730 ksi | ASTM D638 |
LNP Lubricomp® QFL-4017 ER HS Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant
(discontinu Features: Heat Stabilized, Good Mold Release, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; .. |
|||
Tensile Modulus | 11.9 GPa | 1730 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® SK695FR BK507 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK695FR is a 30% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided b.. |