Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 1180 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 8.13 GPa
1180 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM UC1200 PEI (Asia Pacific)
12% carbon fiber reinforced Polyetherimide (Tg 217C). ECO Conforming. UL94 V0 listing in recognized colors.
Tensile Modulus 8.17 GPa
1180 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DEL22P PC
LNP STAT-KON* DEL22P is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 10% PTFE. Added features of this material include: Electrically Conductive. Exceptional Processing, Wear..
Tensile Modulus 8.13 GPa
1180 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI
LNP* Stat-kon* Ultem_UC1200 is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications.
Tensile Modulus 8.13 GPa
1180 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI (Europe-Africa-Middle East)
LNP* Stat-kon* Ultem_UC1200 compound is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications.
Tensile Modulus 8.17 GPa
1180 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DEL22P PC (Asia Pacific)
LNP STAT-KON* DEL22P is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Modulus 8.17 GPa
1180 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOTUF VX00585 PA 66
LNP* Thermotuf* VX00585 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.
Tensile Modulus 8.17 GPa
1180 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOTUF VX00585 PA 66 (Asia Pacific)
LNP* Thermotuf* VX00585 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.
Tensile Modulus 8.17 GPa

@Temperature -100 °C
1180 ksi

@Temperature -148 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100ST NC010 Acetal (POM)  (Unverified Data**)
Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST NC010 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part..
Tensile Modulus 8.133 GPa

@Temperature -70.0 °C
1180 ksi

@Temperature -94.0 °F
DAM; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G25HSLR NC010 is a 25% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol..
Tensile Modulus 8.16 GPa
1180 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Verton PV007SV_WH8D537 PA 6
Preliminary data for 35% long fiber single pellet color filled PA6This data was supplied by SABIC-IP for the Americas region.
Copyright © lookpolymers.com All Rights Reserved