Tensile Strength, Yield | 35.0 - 62.0 MPa | 5080 - 8990 psi | Average value: 52.4 MPa Grade Count:19 |
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an.. |
|||
Tensile Strength, Yield | 39.0 - 62.0 MPa | 5660 - 8990 psi | Average value: 49.7 MPa Grade Count:6 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |
|||
Tensile Strength, Yield | 26.0 - 62.0 MPa | 3770 - 8990 psi | Average value: 42.5 MPa Grade Count:4 |
Overview of materials for Nylon 6/69 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6/69". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Tensile Strength, Yield | 39.0 - 62.0 MPa | 5660 - 8990 psi | Average value: 51.3 MPa Grade Count:4 |
Overview of materials for Acrylic, Impact Modified Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified Sheet". Each property range of values reported is minimum and maximum values of.. |