Polymer Property : Tensile Strength, Yield = 88000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 510 - 607 MPa
74000 - 88000 psi
0.2% offset
Eagle Brass 510 Phosphor Bronzes 5% A, Hard
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
Tensile Strength, Yield 538 - 607 MPa
78000 - 88000 psi
0.2% offset
Eagle Brass 715 Copper Nickel 30%, Extra Hard
715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co..
Tensile Strength, Yield 503 - 607 MPa
73000 - 88000 psi
0.2% offset
Eagle Brass 725 Copper Nickel Tin, Hard
Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina..
Tensile Strength, Yield 414 - 607 MPa
60000 - 88000 psi
0.2% offset
Eagle Brass 762 Nickel Silver 12%, 1/2 Hard
762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s..