Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 510 - 730 MPa | 74000 - 106000 psi | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; H (TD04) Temper; over 25 to 51 mm Thickness (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 510 - 730 MPa | 74000 - 106000 psi | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; H (TD04) Temper; over 51 to 76 mm Thickness (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 510 - 730 MPa | 74000 - 106000 psi | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; H (TD04) Temper; over 9.5 to 25 mm Thickness (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 510 - 730 MPa | 74000 - 106000 psi | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; H (TD04) Temper; up to 9.5 mm Thickness (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 510 - 730 MPa | 74000 - 106000 psi | |
Materion Beryllium Copper Alloy 165 Rod and Bar; H (TD04) Temper; over 25.4 to 76 mm (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 510 - 730 MPa | 74000 - 106000 psi | |
Materion Beryllium Copper Alloy 165 Rod and Bar; H (TD04) Temper; over 9.5 to 25.4 mm (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 510 - 730 MPa | 74000 - 106000 psi | |
Materion Beryllium Copper Alloy 165 Rod and Bar; H (TD04) Temper; up to 9.5 mm (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 510 - 730 MPa | 74000 - 106000 psi | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; H (TD04) Temper; over 51 to 76 mm Thickness (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 510 - 730 MPa | 74000 - 106000 psi | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; H (TD04) Temper; over 9.5 to 25 mm Thickness (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 510 - 730 MPa | 74000 - 106000 psi | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; H (TD04) Temper; up to 9.5 mm Thickness (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 510 - 730 MPa | 74000 - 106000 psi | |
Materion Beryllium Copper Alloy 25 Rod and Bar; H (TD04) Temper; over 9.5 to 25.4 mm (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 510 - 730 MPa | 74000 - 106000 psi | |
Materion Beryllium Copper Alloy 25 Tube; H (TD04) Temper; 0ver 25.4 to 76 mm o.d. (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 510 - 730 MPa | 74000 - 106000 psi | |
Materion Beryllium Copper Alloy 25 Tube; H (TD04) Temper; over 9.5 to 25.4 mm o.d. (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 510 - 730 MPa | 74000 - 106000 psi | |
Materion Beryllium Copper Alloy 25 Tube; H (TD04) Temper; up to 9.5 mm o.d. (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 510 - 670 MPa | 74000 - 97200 psi | |
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM00 Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 76%Formability Ratio, 90° Bend, R.. |
|||
Tensile Strength, Yield | 510 - 730 MPa | 74000 - 106000 psi | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; H (TD04) Temper; over 25 to 51 mm Thickness (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 510 - 730 MPa | 74000 - 106000 psi | |
Materion Beryllium Copper Alloy M25 Rod and Bar; H (TD04) Temper; over 25.4 to 76 mm (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 510 - 730 MPa | 74000 - 106000 psi | |
Materion Beryllium Copper Alloy M25 Rod and Bar; H (TD04) Temper; over 9.5 to 25.4 mm (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 510 - 690 MPa | 74000 - 100000 psi | |
Materion Brush 1915™ Heat Treated Temper Wire, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee.. |
|||
Tensile Strength, Yield | 510 MPa @Strain 0.200 % |
74000 psi @Strain 0.200 % |
|
Haynes 188 alloy, plate at RT after 8000 hours at 760°C (1400°F) Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Tensile Strength, Yield | 510 MPa @Strain 0.200 % |
74000 psi @Strain 0.200 % |
Typical |
TIMET TIMETAL® 230 Titanium Alloy (Ti-2.5Cu); Annealed Cold Formable Medium-Strength AlloyIndustry Specifications: Germany Aerospace: 3.7124. France: T-U2. UK Aerospace Specifications BA TA. 21, 22, 23.Features: This binary, age hardening alloy combi.. |
|||
Tensile Strength, Yield | >= 510 MPa | >= 74000 psi | 0.2% offset |
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Spring 19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect.. |
|||
Tensile Strength, Yield | 510 - 607 MPa | 74000 - 88000 psi | 0.2% offset |
Eagle Brass 510 Phosphor Bronzes 5% A, Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Tensile Strength, Yield | 510 - 579 MPa | 74000 - 84000 psi | 0.2% offset |
Eagle Brass 735 Nickel Silver 18%, Spring 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |
|||
Tensile Strength, Yield | >= 510 MPa @Strain 0.200 % |
>= 74000 psi @Strain 0.200 % |
|
CLAL-MSX NICLAFOR® 1000 TF Quenched/Precipitation Heat Treated, Rolled Copper Alloy Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi.. |
|||
Tensile Strength, Yield | 510 MPa @Strain 0.200 % |
74000 psi @Strain 0.200 % |
|
AK Steel 2205 Duplex Stainless steel AK Steel 2205 provides a combination of high strength, excellent corrosion resistance and stress-corrosion cracking resistance as well as very good pitting resistance, and low thermal expansion. Th.. |
|||
Tensile Strength, Yield | 510 - 560 MPa | 74000 - 81200 psi | L direction |
ArcelorMittal Speed 35-510 Electrical Steel Properties: The iCARe™ Speed product family comes with guaranted losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie.. |
|||
Tensile Strength, Yield | 510 MPa @Strain 0.200 % |
74000 psi @Strain 0.200 % |
|
Haynes Hastelloy® C-22® alloy, all-weld metal, SMAW HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Tensile Strength, Yield | 510 MPa @Strain 0.200 % |
74000 psi @Strain 0.200 % |
|
Haynes Hastelloy® C-22® alloy, GTAW weld, 904L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Tensile Strength, Yield | 510 MPa @Strain 0.200 % |
74000 psi @Strain 0.200 % |
|
Haynes 25 alloy, room temperature after 10% cold reduction, 1120°C anneal for 5 minutes Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall.. |