Tensile Strength, Yield 503 MPa

@Strain 0.200 %
73000 psi

@Strain 0.200 %
Haynes Hastelloy® C-22® alloy, SMAW weld, 316L base metal, C-22 weld metal
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Tensile Strength, Yield 503 MPa
73000 psi
Universal Wire Works 617 Nickel Alloy Welding Wire
Alloy 617 is used for TIG and MIG welding of Inconel type alloy 617 and alloys of similar composition. Alloy 617 welds produce high stress-rupture strength in prolonged exposure to high temperatures..
Tensile Strength, Yield 503 - 552 MPa
73000 - 80000 psi
0.2% offset
Eagle Brass 230 Red Brass, Extra Spring
CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste..
Tensile Strength, Yield 503 - 579 MPa
73000 - 84000 psi
0.2% offset
Eagle Brass 240 Low Brass, Extra Spring
CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib..
Tensile Strength, Yield 503 - 586 MPa
73000 - 85000 psi
0.2% offset
Eagle Brass 425 Tin Brass 2%, Extra Hard
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
Tensile Strength, Yield 503 - 621 MPa
73000 - 90000 psi
0.2% offset
Eagle Brass 519 Phosphor Bronzes 6%, Hard
Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C..
Tensile Strength, Yield 503 - 579 MPa
73000 - 84000 psi
0.2% offset
Eagle Brass 715 Copper Nickel 30%, Hard
715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co..
Tensile Strength, Yield 503 - 607 MPa
73000 - 88000 psi
0.2% offset
Eagle Brass 725 Copper Nickel Tin, Hard
Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina..
Tensile Strength, Yield 503 - 627 MPa
73000 - 91000 psi
0.2% offset
Eagle Brass 762 Nickel Silver 12%, 3/4 Hard
762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s..