Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 827 MPa | 120000 psi | |
Pacific Sintered Materials FX-232-T(HT) Infiltrated High Carbon Steel Powdered Metal Good strength, shock resistance and hardenability. Moderate tolerance control.Equivalent MPIF Specification: FX-1008-110HTAll information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | >= 827 MPa | >= 120000 psi | 0.2% proof |
Kobe Steel KS6-2-4-2 Alpha Titanium Alloy, AMS 4976, Solution treated and aged Nominal Composition: Ti-6 Al-2 Sn-4 Zr-2 Mo Applications: Jet engine parts, engine valves.Features:Heat resistant. Information provided by Kobe Steel |
|||
Tensile Strength, Yield | 827 - 1030 MPa @Strain 0.200 % |
120000 - 150000 psi @Strain 0.200 % |
|
Materion BrushCAST® 20C High Strength Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 827 - 1030 MPa @Strain 0.200 % |
120000 - 150000 psi @Strain 0.200 % |
|
Materion BrushCAST® 21C High Strength Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Yield | >= 827 MPa @Strain 0.200 % |
>= 120000 psi @Strain 0.200 % |
|
Materion ToughMet® T3 AT120 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Tensile Strength, Yield | >= 827 MPa @Strain 0.200 % |
>= 120000 psi @Strain 0.200 % |
|
Materion ToughMet® T3 AT120 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Tensile Strength, Yield | 827 MPa | 120000 psi | Up to 1.5 inches; Un-Nitrided |
Latrobe LSSâ„¢ 135M Nitriding Steel (ASTM A355 Class A) TLS 135M Nitriding Steel is a high-aluminum and chromium modification of AISI 4140 alloy steel. The aluminum addition promotes the formation of aluminum nitride compounds when tools manufactured fr.. |
|||
Tensile Strength, Yield | >= 827 MPa | >= 120000 psi | |
Materion Alloy M65 (C17465) Beryllium Copper Rod Alloy M65 (C17465) is a machinable, high-performance, copper beryllium rod alloy from Brush Wellman. M65 has excellent strength, conductivity, and resistance to elevated temperature stress relaxatio.. |
|||
Tensile Strength, Yield | 827 - 1069 MPa | 120000 - 155000 psi | |
Materion Beryllium Nickel Strip - Alloy 360 MH4, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Tensile Strength, Yield | 827 - 1030 MPa @Strain 0.200 % |
120000 - 150000 psi @Strain 0.200 % |
|
Materion BrushCAST® 20CT Fine Grain Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 827 MPa @Strain 0.200 % |
120000 psi @Strain 0.200 % |
|
Special Metals INCOLOY® alloy 908 INCOLOY® alloy 908 (UNS N09908) is an age-hardenable nickel-iron alloy which exhibits a low coefficient of thermal expansion, high tensile strength, high fracture and impact toughness, fatigue cr.. |
|||
Tensile Strength, Yield | 827 MPa @Strain 0.200 % |
120000 psi @Strain 0.200 % |
|
Special Metals INCONEL® 718SPF™ Nickel Superalloy, Annealed Typical annealing - continuous process anneal, 1700°F (927°C) at 15 ft (4.57 m) per minute. This produces ASTM No. 12 grain size. Heat capacity, melting range, moduli, and Poisson's ratio re.. |
|||
Tensile Strength, Yield | 827 MPa @Strain 0.200 % |
120000 psi @Strain 0.200 % |
|
Universal Wire Works 6Al-4V (AMS 4954) Titanium Alloy Filler Metal Universal 6Al-4V titanium alloy is often repaired with the gas tungsten arc or gas metal arc welding process, provided adequate inert gas shielding of the filler wire and deposited weld metal is pro.. |
|||
Tensile Strength, Yield | 827 MPa @Strain 0.200 % |
120000 psi @Strain 0.200 % |
|
Universal Wire Works 6Al-4V (ELI) (AMS 4956) Titanium Alloy Filler Metal Universal titanium alloy 6Al-4V (ELI) is similar to type 6Al-4V in chemical analysis with the exception of Extra Low Interstitial gases (ELI). By controlling these contaminating gases the fracture t.. |
|||
Tensile Strength, Yield | >= 827 MPa @Strain 0.200 % |
>= 120000 psi @Strain 0.200 % |
|
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness, Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness, |
|||
Tensile Strength, Yield | >= 827 MPa @Strain 0.200 % |
>= 120000 psi @Strain 0.200 % |
|
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness, 4.00-6.00 in, Annealed, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness, 4.00-6.00 in, Annealed, Per Mil-T-9047G; other specific form/thickness entries .. |
|||
Tensile Strength, Yield | 827 MPa @Strain 0.200 % |
120000 psi @Strain 0.200 % |
|
ECOMold 95 Copper Mold Material ECOMold® copper alloys (beryllium-free) are designed specifically for plastics industry applications. ECOMold® 95 has a superior combination of thermal conductivity, hardness, and tensile strengt.. |
|||
Tensile Strength, Yield | 827 MPa @Strain 0.200 % |
120000 psi @Strain 0.200 % |
|
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 48% Cold Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Tensile Strength, Yield | 827 - 930 MPa @Strain 0.200 % |
120000 - 135000 psi @Strain 0.200 % |
|
Ametek AM 388™ Alloy (UNS C72650) TS02 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Tensile Strength, Yield | 827 MPa @Strain 0.200 % |
120000 psi @Strain 0.200 % |
|
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 718°C (1325°F)/8hr/AC to 621°C (1150°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Tensile Strength, Yield | 827 MPa | 120000 psi | 9.4% cold reduction |
ATI Allegheny Ludlum AL 2003™ Duplex Stainless Steel Characteristics: superior stress corrosion cracking resistance to Types 316 and 317, yield strength double that of conventional austenitic stainless steel, good corrosion resistance, good chloride s.. |
|||
Tensile Strength, Yield | 827 MPa @Temperature 427 °C |
120000 psi @Temperature 801 °F |
40% Cold Worked |
ATI Allegheny Ludlum Allcorr® Nickel-Based, Corrosion Resistant Alloy Characteristics: non-age hardenable; outstanding resistance to general corrosion, pitting corrosion, crevice corrosion, intergranular corrosion, and stress corrosion cracking; high strength; high du.. |