ATI Allegheny Ludlum Allcorr® Nickel-Based, Corrosion Resistant Alloy

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer ATI Allegheny Ludlum
Trade Name Allcorr®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allegheny Ludlum Allcorr® Nickel-Based, Corrosion Resistant Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: non-age hardenable; outstanding resistance to general corrosion, pitting corrosion, crevice corrosion, intergranular corrosion, and stress corrosion cracking; high strength; high ductility, good weldability; good hot and cold workability; good machinabilityInformation provided by Allegheny Ludlum
Physical Properties Metric English Comments
Density 8.327 g/cc
0.3008 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 310 MPa
45000 psi
Annealed
1010 MPa
146000 psi
40% Cold Worked
207 MPa

@Temperature 427 °C
30000 psi

@Temperature 801 °F
Annealed
827 MPa

@Temperature 427 °C
120000 psi

@Temperature 801 °F
40% Cold Worked
Elongation at Break 20 %
20 %
Annealed
70 %
70 %
40% Cold Worked
20 %

@Temperature 427 °C
20 %

@Temperature 801 °F
Annealed
79 %

@Temperature 427 °C
79 %

@Temperature 801 °F
40% Cold Worked
Thermal Properties Metric English Comments
CTE, linear 12.0 µm/m-°C

@Temperature 20.0 - 100 °C
6.67 µin/in-°F

@Temperature 68.0 - 212 °F
13.0 µm/m-°C

@Temperature 20.0 - 400 °C
7.22 µin/in-°F

@Temperature 68.0 - 752 °F
15.1 µm/m-°C

@Temperature 20.0 - 800 °C
8.39 µin/in-°F

@Temperature 68.0 - 1470 °F
Specific Heat Capacity 0.421 J/g-°C

@Temperature 20.0 °C
0.101 BTU/lb-°F

@Temperature 68.0 °F
0.478 J/g-°C

@Temperature 300 °C
0.114 BTU/lb-°F

@Temperature 572 °F
0.530 J/g-°C

@Temperature 600 °C
0.127 BTU/lb-°F

@Temperature 1110 °F
0.582 J/g-°C

@Temperature 1000 °C
0.139 BTU/lb-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
Aluminum, Al 0.25 %
0.25 %
Carbon, C 0.010 %
0.010 %
Chromium, Cr 30 %
30 %
Molybdenum, Mo 11 %
11 %
Nickel, Ni >= 56.39 %
>= 56.39 %
Niobium, Nb (Columbium, Cb) 0.10 %
0.10 %
Titanium, Ti 0.25 %
0.25 %
Tungsten, W 2.0 %
2.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.000122 ohm-cm

@Temperature 20.0 °C
0.000122 ohm-cm

@Temperature 68.0 °F