Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 760 MPa
>= 110000 psi
MetalTek IN® 718 UNS N07718 Centri-Vac Nickel Cobalt Based Alloy
Information provided by MetalTek
Tensile Strength, Yield >= 760 MPa
>= 110000 psi
MetalTek MTEK 718 Cast UNS N07718 Severe Corrosion and Heat Resistant Alloy
Information provided by MetalTek
Tensile Strength, Yield >= 760 MPa
>= 110000 psi
MetalTek RENE® 77 Centri-Vac Nickel Cobalt Based Alloy
Information provided by MetalTekWrought Grade RENE® 77
Tensile Strength, Yield 760 MPa

@Strain 0.200 %
110000 psi

@Strain 0.200 %
Haynes 242® alloy
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Tensile Strength, Yield 760 MPa

@Strain 0.200 %,
Temperature 95.0 °C
110000 psi

@Strain 0.200 %,
Temperature 203 °F
Haynes 242® alloy, bar and rings, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Tensile Strength, Yield 760 MPa

@Strain 0.200 %,
Temperature 650 °C
110000 psi

@Strain 0.200 %,
Temperature 1200 °F
Precipitation Hardened prior to test
Special Metals INCONEL® Alloy 751
A nickel-chromium alloy similar to INCONEL ALLOY X-750 but with increased aluminum content for greater precipitation hardening. INCONEL alloy 751 was designed for use as exhaust valves in internal-..
Tensile Strength, Yield 760 MPa

@Strain 0.200 %,
Temperature 550 °C
110000 psi

@Strain 0.200 %,
Temperature 1020 °F
Precipitation Hardened prior to test
Special Metals INCONEL® Alloy X-750
A nickel-chromium alloy similar to INCONEL alloy 600 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good resistance to corrosion and oxidation along with hig..
Tensile Strength, Yield 760 MPa

@Strain 0.200 %
110000 psi

@Strain 0.200 %
Precipitation Hardened
Special Metals NI-SPAN-C® Alloy 902
A nickel-iron-chromium alloy made precipitation hardenable by additions of aluminum and titanium. The titanium content also helps provide a controllable thermoelastic coefficient, which is the allo..
Tensile Strength, Yield >= 760 MPa

@Strain 0.200 %
>= 110000 psi

@Strain 0.200 %
L and LT Directions
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; 1.75 - 2.50 in Rod or Thickness; Per ASTM F136)
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A..
Tensile Strength, Yield >= 760 MPa

@Strain 0.200 %
>= 110000 psi

@Strain 0.200 %
L, LT and ST Directions
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; 2.50 - 4.00 in Rod or Thickness; Per ASTM F136)
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A..
Tensile Strength, Yield 760 - 830 MPa

@Strain 0.200 %
110000 - 120000 psi

@Strain 0.200 %
CLAL-MSX DECLAFOR® 1015 TH2 Wire quenched/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Tensile Strength, Yield 760 MPa
110000 psi
Elgiloy® Co-Cr-Ni Alloy, Wire, 10% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi..
Tensile Strength, Yield 760 MPa

@Strain 0.200 %
110000 psi

@Strain 0.200 %
Carpenter Pyromet® CTX-3 Superalloy, Heat Treatment for Brazing Cycles over 982°C
Data provided by Carpenter Technology Corporation.Pyromet® alloy CTX-3 is a high strength, precipitation hardenable superalloy which exhibits a low CTE over a broad temperature range. This alloy a..
Tensile Strength, Yield 760 MPa

@Strain 0.200 %
110000 psi

@Strain 0.200 %
ATI Allegheny Ludlum AL 17-4 High Strength Stainless Steel, UNS S17400
Property data below is typical of annealed samples. Available in plate. For use in fasteners, fittings, military equipment and air frame parts.Information provided by Allegheny Ludlum
Tensile Strength, Yield 760 MPa

@Strain 0.200 %
110000 psi

@Strain 0.200 %
ATI Allegheny Ludlum AL 15-5 High Strength Stainless Steel, UNS S15500
Property data below is typical of annealed samples. Available in plate. For use in fasteners, military equipment and air frame parts.Information provided by Allegheny Ludlum
Tensile Strength, Yield 760 MPa

@Strain 0.200 %
110000 psi

@Strain 0.200 %
Carpenter BioDur™ CCM® Medical Implant Alloy, Hot Worked
Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur Carpenter CCM alloy..