MetalTek RENE® 77 Centri-Vac Nickel Cobalt Based Alloy

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer MetalTek
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek RENE® 77 Centri-Vac Nickel Cobalt Based Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MetalTekWrought Grade RENE® 77
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 860 MPa
>= 125000 psi
Tensile Strength, Yield >= 760 MPa
>= 110000 psi
Component Elements Properties Metric English Comments
Aluminum, Al 4.0 - 4.6 %
4.0 - 4.6 %
Carbon, C 0.050 - 0.090 %
0.050 - 0.090 %
Chromium, Cr 14 - 15.25 %
14 - 15.25 %
Cobalt, Co 14.25 - 15.75 %
14.25 - 15.75 %
Molybdenum, Mo 3.9 - 4.5 %
3.9 - 4.5 %
Nickel, Ni 56.11 - 60.8 %
56.11 - 60.8 %
As Balance
Titanium, Ti 3.0 - 3.7 %
3.0 - 3.7 %
Descriptive Properties Value Comments
Heat Treatment Sol. Anneal & Age