Polymer Property : Tensile Strength, Yield = 660 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.55 MPa
660 psi
-30% change after 336 hours @ 200°C; ASTM D412
Precision Polymer Engineering F80R Fluorosilicone Rubber
Red Fluorosilicone, 76-85 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification DTD5583A Grade 80.Applications:
Tensile Strength, Yield 4.55 MPa
660 psi
200%, post cured- 8 hours at 177°C; ASTM D412
Multibase C6-265 DI-CUP R Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 4.55 MPa
660 psi
200%, post cured- 8 hours at 177°C; ASTM D412
Multibase C6-265 VAROX DBPH Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 4.55 MPa
660 psi
at 100% secant; ASTM D638
Multibase Multi-Flex® A 8502 LC TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Thermal Stability, GoodOzone Resistant Forms:PelletsProcessing Method:Injection MoldingExtrusion Uses: Automotive Interior PartsInformation provided by Multiba..
Tensile Strength, Yield 4.55 MPa

@Strain 100 %
660 psi

@Strain 100 %
ASTM D412
Multibase Multi-Flex® A 8502 LC UV RXF/YYWA Black TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Tensile Strength, Yield 4.55 MPa
660 psi
ASTM D638
ExxonMobil Escorene™ LD 723.28 Molding Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra LD 723.28 is a 18.5 wt% vinyl acetate copolymer suitable for injection molding and compounding applications.Availability: Latin America, North America and South A..