Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.55 MPa | 660 psi | -30% change after 336 hours @ 200°C; ASTM D412 |
Precision Polymer Engineering F80R Fluorosilicone Rubber Red Fluorosilicone, 76-85 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification DTD5583A Grade 80.Applications: |
|||
Tensile Strength, Yield | 4.55 MPa | 660 psi | 200%, post cured- 8 hours at 177°C; ASTM D412 |
Multibase C6-265 DI-CUP R Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 4.55 MPa | 660 psi | 200%, post cured- 8 hours at 177°C; ASTM D412 |
Multibase C6-265 VAROX DBPH Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 4.55 MPa | 660 psi | at 100% secant; ASTM D638 |
Multibase Multi-Flex® A 8502 LC TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Thermal Stability, GoodOzone Resistant Forms:PelletsProcessing Method:Injection MoldingExtrusion Uses: Automotive Interior PartsInformation provided by Multiba.. |
|||
Tensile Strength, Yield | 4.55 MPa @Strain 100 % |
660 psi @Strain 100 % |
ASTM D412 |
Multibase Multi-Flex® A 8502 LC UV RXF/YYWA Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tensile Strength, Yield | 4.55 MPa | 660 psi | ASTM D638 |
ExxonMobil Escorene™ LD 723.28 Molding Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 723.28 is a 18.5 wt% vinyl acetate copolymer suitable for injection molding and compounding applications.Availability: Latin America, North America and South A.. |