Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 52.0 - 56.0 MPa | 7540 - 8120 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 3208/0150 Anti-friction PVDF Compound
(discontinued **) Key features of this grade: Anti-friction, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |
|||
Tensile Strength, Yield | 25.0 - 56.0 MPa | 3630 - 8120 psi | Average value: 39.7 MPa Grade Count:10 |
Overview of materials for Nylon 11, Cable Sheathing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Cable Sheathing Grade". Each property range of values reported is minimum and maximum values o.. |
|||
Tensile Strength, Yield | 55.0 - 56.0 MPa | 7980 - 8120 psi | ASTM D638M |
DSM Somos® WaterClear® Ultra 10122 Optically Clear, Colorless, Rigid, Stereolithography Resin DescriptionDSM Somos® WaterClear Ultra 10122 is a next generation optically clear resin with ABS like properties and good temperature resistance. It produces colorless, functional, accurate parts .. |
|||
Tensile Strength, Yield | 47.0 - 56.0 MPa | 6820 - 8120 psi | Typical |
ATI Allegheny Ludlum AL 20™ Sheet and Strip Specialty Steel The N08020 alloy has been available for many years and has found applications in many environments, such as in chlorides and in sulfuric and sulfurous acids.Although AL 20 alloy was developed for im.. |