Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering F80X Fluorosilicone Rubber

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering F80X Fluorosilicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mid-Blue Fluorosilicone Rubber, 76-85 °IRHD . Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification Mil-R-25988B, Class 1, Grade 80.Applications: Intended for use in applications where resistance to jet fuels, hydraulic fluids, lubricants, silicone and ester-based fluids (but excluding certain phosphate esters) is required.
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
°IRHD; ASTM D1415
75 - 90
75 - 90
°IRHD, +10/-5 change after 70 hours @ 200°C; ASTM D1415
Tensile Strength, Yield 4.16 MPa
603 psi
-20% change after 70 hours @ 200°C; ASTM D412
5.20 MPa
754 psi
ASTM D412
Elongation at Break 56 %
56 %
-20% change after 70 hours @ 200°C; ASTM D412
70 %
70 %
ASTM D412
Compression Set 40 %
40 %
22 hours @ 175°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
-57.0 °C
-70.6 °F
TR10
Flash Point >= 300 °C
>= 572 °F