ACC QM260 Addition Cure 2-Part Molding Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Amber Chemical Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ACC QM260 Addition Cure 2-Part Molding Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: cures at room temperature, low shrinkage, high tear and tensile strengths. Applications: expanded PU foam, large objects.
Physical Properties Metric English Comments
Viscosity 105000 cP
105000 cP
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Tensile Strength, Yield 5.20 MPa
754 psi
Elongation at Break 190 %
190 %
Tear Strength 14.8 kN/m
84.4 pli
Descriptive Properties Value Comments
Color Light Blue