Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 32.0 - 32.0 MPa @Temperature 100 - 100 °C |
4640 - 4640 psi @Temperature 212 - 212 °F |
Average value: 32.0 MPa Grade Count:1 |
Overview of materials for Polyphthalamide (PPA), High Impact This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, High Impact". Each property range of values reported is minimum and maximum values of a.. |
|||
Tensile Strength, Yield | 14.0 - 32.0 MPa | 2030 - 4640 psi | Average value: 25.1 MPa Grade Count:55 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Tensile Strength, Yield | 30.0 - 32.0 MPa | 4350 - 4640 psi | ASTM D638M |
DSM Somos® 9120 Epoxy Photopolymer
(Unverified Data**) DescriptionDSM Somos® 9120 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance, a wide p.. |