Mechanical Properties Metric English Comments
Tensile Strength, Yield 38.0 - 44.0 MPa
5510 - 6380 psi
ASTM D638
3D Systems Accura® Xtreme Plastic for SLA® Systems
For use with solid-state stereolithography (SLA®) systemsApplicationsForm, fit and function prototypesDurable AssembliesSnap fit assembliesTough enclosuresConsumer electronic componentsMaster patte..
Tensile Strength, Yield 41.0 - 44.0 MPa
5950 - 6380 psi
Addcomp PRIEX® Ionomer 42101 PP homopolymer
Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t..
Tensile Strength, Yield 41.0 - 44.0 MPa
5950 - 6380 psi
Addcomp PRIEX® Ionomer 40101 PP homopolymer
Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t..
Tensile Strength, Yield 15.0 - 44.0 MPa
2180 - 6380 psi
Average value: 35.1 MPa Grade Count:25
Overview of materials for Nylon 11, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..