Material Notes:
CHARACTERISTICS: HIGH CLARITY, HIGH IMPACT, GOOD EXTRUDABILITY APPLICATIONS: BLOW MOLDING, SHEET EXTRUSION FOR COSMETIC BOTTLES, SHEET FOR THERMOFORMING, CLOSURES, FILES
Physical Properties Metric English Comments
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 29.5 MPa
4280 psi
ASTM D638
Elongation at Yield 38 %
38 %
ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
1% Secant; ASTM D790
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.24 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Heat Distortion Temperature 83.0 °C
181 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 170 - 230 °C
338 - 446 °F