Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 36.3 MPa | 5260 psi | ASTM D638 |
PolyMirae Moplen HF524J BDDP Film Grade Polypropylene Moplen HF524J is the Addiform polypropylene. Compared to ordinary pelletized polypropylene, Addiform gives significant advantages in terms of improved productivity, better processing and lower energ.. |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | ASTM D638 |
PolyMirae Moplen HF550K Stretch/Yarn, Monofilament Grade Polypropylene Moplen HF550K is the ADDIFORM polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Its appearance is spherical, white particle with diameter of 1mm .. |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | ASTM D638 |
PolyMirae Moplen HP525J BDDP Film Grade Polypropylene Moplen HP525J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP525J is a homopolymer particularly suitable for Metallizable BOPP.. |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | ASTM D638 |
PolyMirae Moplen HP557G Stretch Grade Polypropylene Moplen HP557G is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP557G is a homopolymer suitable for high strength rope, container .. |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | ASTM D638 |
PolyMirae Moplen HP600R Injection Grade Polypropylene Moplen HP600R is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP600R is a homopolymer typically used in injection molding of food.. |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | ASTM D638 |
PolyMirae Moplen HP740T Injection Molding (Thin Wall) Grade Polypropylene Moplen HP740T is a nucleated polypropylene HOMO polymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP740T is a homopolymer selected by customers for use in t.. |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | ASTM D638 |
PolyMirae Moplen HP425J BDDP Film Grade Polypropylene Moplen HP425J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. MIRAEPOL T28C is a homopolymer particularly suitable for BOPP (Tender) fil.. |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | ASTM D638 |
PolyMirae Moplen HP450J Stretch/Yarn, Monofilament Grade Polypropylene Moplen HP450J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP450J is a homopolymer typically used by customers in Raffia and Y.. |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | ASTM D638 |
PolyMirae Moplen HP500G Sheet and Thermoforming Grade Polypropylene Moplen HP500G is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP500G is a homopolymer particularly suitable for sheet, thermofor.. |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | ASTM D638 |
Hyosung Topilene F600 PP F600 Film Grade HomopolymerApplications: IPPCharacteristics:ProcessabilityTransparencyInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | ASTM D638 |
Hyosung Topilene F603 PP F603 Film Grade HomopolymerApplications: CPPCharacteristics:ProcessabilityTransparencystiffnessInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | ASTM D638 |
Hyosung Topilene J700 PP J700 Injection General HomopolymerApplications: General injectionCharacteristics:ProcessabilityStiffnessInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | ASTM D638 |
Hyosung Topilene S700 PP S700 Fiber Grade HomopolymerApplications:Continuous filamentBCFCharacteristics:ProcessabilityInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | ASTM D638 |
Hyosung Topilene S800 PP S800 Injection Special Purpose GradeApplications:Electric home applianceHousewares applianceCharacteristics:Heat resistanceInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | ASTM D638 |
Hyosung Topilene S800F PP S800F Fiber Grade HomopolymerApplications:Staple fiberBCFFine denier filamentCharacteristics:ProcessabilityInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 36.3 MPa @Thickness 3.20 mm |
5260 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical ALPHALAC SG960 HIPS Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Washer Cover, Air-conditioner Panel, Refrigerator PartsCAS No. 9003-55-8Information provided by LG Chemical |
|||
Tensile Strength, Yield | 36.3 MPa @Thickness 3.20 mm |
5260 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL GP3200 PP+MF20% Description: Injection Molding, PP+MF10%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | 50 mm/min; ASTM D638 |
LG Chemical MI-770 MIPS |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | ASTM D638 |
Lotte Chemical Titan TITANPRO® PD855 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | ASTM D638 |
IRPC Polimaxx Polene 111JX TA8 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE HOMOPOLYMER WITH 40% TALCUM REINFORCED HIGH STIFFNESSAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | ASTM D638 |
Hyosung Topilene J800 PP J800 Injection General HomopolymerApplications: General injectionCharacteristics:FlowabilityStiffnessInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | ASTM D638 |
Hyosung Topilene J800R PP J800R Injection Special Purpose GradeApplications:Electric home applianceHousewares applianceCharacteristics:Long-term heat resistanceInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 36.3 MPa @Thickness 3.20 mm |
5260 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical AF360 ABS, TBBA-free Flame Retardant Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b.. |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | 50 mm/min; ASTM D638 |
LG Chemical SG-950 Alphalac Polystyrene High strength, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electr.. |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | ASTM D638 |
IRPC Polimaxx Polene 1111NX TA4 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE HOMOPOLYMER WITH 20% TALCUM REINFORCEDAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SP-0180 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SP-0180 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | ASTM D638 |
SCG Chemicals EL-Leneâ„¢ H6240B High Density Polyethylene Blow Molding Key Characteristics:Good stiffnessGood environmental stress cracking resistance (ESCR)High compressive and impact strengthGood appearanceOdorlessSafe for food contactGood printabilityRecommended App.. |
|||
Tensile Strength, Yield | 36.3 MPa | 5260 psi | ASTM D638 |
SCG Chemicals EL-Leneâ„¢ H6430BM High Density Polyethylene Blow Molding Key Characteristics:Excellent stiffnessGood processabilityOdorlessSafe for food contactGood printabilityRecommended Applications:Bottles for drinking water, fruit juice, soft drink, milkAutomotive p.. |