Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyMirae Moplen HP740T Injection Molding (Thin Wall) Grade Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer PolyMirae Company Ltd.
Trade Name Moplen
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyMirae Moplen HP740T Injection Molding (Thin Wall) Grade Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Moplen HP740T is a nucleated polypropylene HOMO polymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP740T is a homopolymer selected by customers for use in thin wall injection molding for packaging, food tray. Moplen HP740T meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520 for food contact.Features: Outstanding Flowability; Excellent Transparency and Gloss; High stiffness; Good transparency Applications: Food Tray; Plastic file; Drinking cup; TWIM; DVD CaseInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D1505
Melt Flow 60 g/10 min

@Load 2.16 kg,
Temperature 230 °C
60 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.77 GPa
256 ksi
ASTM D790
Izod Impact, Notched 0.226 J/cm
0.422 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
ASTM D648