Material Notes:
Moplen HP557G is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP557G is a homopolymer suitable for high strength rope, container bags and extruded nets. Moplen HP557G resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 178.2010 for food packaging substances with adequate additives. And contains no dangerous substances according to Federal Regulations in 21 CFR 177.1520. Features: High mechanical properties; Good UV stabilityApplications: High strength for container bag; Rope; Extruded netsInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 1.3 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.3 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
Izod Impact, Notched 0.588 J/cm
1.10 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 103 °C
217 °F
ASTM D648
Vicat Softening Point 152 °C
306 °F
ASTM D1525
Users viewing this material also viewed the following: