SCG Chemicals EL-Leneâ„¢ H6430BM High Density Polyethylene Blow Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer SCG Chemicals Co.
Trade Name EL-Lene™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SCG Chemicals EL-Leneâ„¢ H6430BM High Density Polyethylene Blow Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Characteristics:Excellent stiffnessGood processabilityOdorlessSafe for food contactGood printabilityRecommended Applications:Bottles for drinking water, fruit juice, soft drink, milkAutomotive parts such as radiator, mirror cleaning pot, ice box, coolerInformation provided by SCG Chemicals
Physical Properties Metric English Comments
Specific Gravity 0.966 g/cc
0.966 g/cc
ASTM D1505
Environmental Stress Crack Resistance 24 hour

@Temperature 50.0 °C
24 hour

@Temperature 122 °F
F50, 25% Igepal; ASTM D1693
Melt Flow 0.40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
ASTM D2240
Tensile Strength at Break 29.0 MPa
4210 psi
ASTM D638
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
Elongation at Break 1200 %
1200 %
ASTM D638
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
Izod Impact, Notched 2.45 J/cm

@Temperature 23.0 °C
4.59 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 132 °C
270 °F
ASTM D2117
Vicat Softening Point 128 °C
262 °F
ASTM D1525
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746