Mechanical Properties Metric English Comments
Tensile Strength, Yield 350 - 440 MPa

@Strain 0.200 %
50800 - 63800 psi

@Strain 0.200 %
SSAB Tunnplat Docol® 350YP High-strength Steel
High-strength SteelComments: Docol YP - Cold Rolled Steel - HSLA. Property values are for cold-rolled steel; thicknesses 0.5 - 3.00 mm. Iron content is approximate - exact composition is not report..
Tensile Strength, Yield 350 - 440 MPa

@Strain 0.200 %
50800 - 63800 psi

@Strain 0.200 %
SSAB Tunnplat Docol® 600DP High-strength Steel
High-strength SteelComments: Docol DP - Cold Rolled Steel - Extra high-strength steel (EHS). Property values are for cold-rolled steel; thicknesses 0.5 - 1.6 mm. Iron content is approximate - exact..
Tensile Strength, Yield 360 - 440 MPa
52200 - 63800 psi
ArcelorMittal Complex Phase Steel 600 Very high strength steel, Cold Rolled Steel
Available in the following: uncoated (HCT600C) and electrogalvanized (HCT600C+ZE)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) product r..