Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 35.1 MPa | 5090 psi | ASTM D638 |
Petromont 5001 High Density Polyethylene Resin Petromont HDPE 5001 is a high-density polyethylene copolymer resin produced using the UNIPOL®
Process. This resin is intended for use in prime sheet and thermoforming applications such as arena boa.. |
|||
Tensile Strength, Yield | 35.1 MPa | 5090 psi | |
Ineos ABS Lustran® 130 Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Injection moldingSheet extrusionBlow moldingThermoforming |
|||
Tensile Strength, Yield | 35.1 MPa | 5090 psi | ASTM D638 |
ExxonMobil PP5722E1 Polypropylene Copolymer Product Description: A medium flow homopolymer resin designed for mono-oriented products like stretched tapes and monofilament.Availability: Asia Pacific Features:Good Gauge ControlGood Processabil.. |
|||
Tensile Strength, Yield | 35.1 MPa | 5090 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 9401 Injection Molding Grade, Ultra High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |