Material Notes:
Product Description: A medium flow homopolymer resin designed for mono-oriented products like stretched tapes and monofilament.Availability: Asia Pacific Features:Good Gauge ControlGood ProcessabilityLow Water CarryoverMedium Flow Uses: FabricsRopeTapeYarn Processing Method: ExtrusionInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.1 MPa
5090 psi
ASTM D638
Elongation at Yield 9.8 %
9.8 %
ASTM D638
Flexural Modulus, 1% Secant 1480 MPa
215000 psi
0.05 in/min; ASTM D790A
1700 MPa
246000 psi
0.5 in/min; ASTM D790B
Izod Impact, Notched 0.395 J/cm
0.740 ft-lb/in
ASTM D256A
Gardner Impact 3.04 J

@Thickness 3.17 mm,
Temperature -28.9 °C
2.24 ft-lb

@Thickness 0.125 in,
Temperature -20.0 °F
Geometry GC; ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.3 °C
200 °F
ASTM D648