Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 310 - 480 MPa | 45000 - 69600 psi | |
Materion Brush 1915â„¢ Hard Temper Rod, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
MetalTek C86200 Med. Tensile Manganese Bronze High strength and hardness copper-zinc alloy.Applications: Steel mill nuts, ordnance parts, worm gears.Information provided by MetalTekCast UNS C86200; Cast Grade C86200; Cast ASTM B271, B584, B148;.. |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
MetalTek MTEK 175-C Cast UNS C95400HT Aluminum Bronze Versatile alloy with high strength, good ductility, unusual toughness, plus exceptional wear resistance. Aluminum Bronze heat treated to higher mechanical properties where necessary.Information prov.. |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
MetalTek MTEK CX-2MW Cast UNS N26022 Severe Corrosion and Heat Resistant Alloy Information provided by MetalTek |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 %, Temperature 427 °C |
45000 psi @Strain 0.200 %, Temperature 801 °F |
|
Haynes Ultimet® alloy, 6.3-38.1 mm plate Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 310 MPa | 45000 psi | |
Mueller Alloy 3530 High Leaded Brass 62% (UNS C35300) Used for screw machine products requiring some cold formability (i.e. crimping, knurling)Applications: Alloy 3530 is used for screw machine applications requiring the ability to be cold formed eithe.. |
|||
Tensile Strength, Yield | 310 MPa | 45000 psi | |
Mueller Alloy 3600 Free Cutting Brass (UNS C36000) Machinability: Recently amended and revised to reflect a lower maximum lead percentage; C36000 remains the industry standard for general machining and high volume production. The excellent machinabi.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 %, Temperature 648 °C |
45000 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes 556® alloy, all-weld metal GTAW Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Yield | 310 - 448 MPa @Strain 0.200 % |
45000 - 65000 psi @Strain 0.200 % |
Magnetically Annealed (Grade 1) |
Schmolz + Bickenbach 430FR Stainless Steel Bar Description: Ugitech’s 430FR is a ferritic stainless steel designed for soft magnetic components operating in corrosive environments. The 17.00% - 18.00% chromium makes corrosion resistance sim.. |
|||
Tensile Strength, Yield | 310 - 379 MPa | 45000 - 55000 psi | 0.2% offset |
Eagle Brass 210 Gilding Metal, 3/4 Hard CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
|
Crucible Steel 430 Chromium Steel Crucible 430 is essentially a non-hardenable chromium steel which is adaptable for general purpose corrosion and heat resisting applications. It is prone to slight hardening by heat treatment. This.. |
|||
Tensile Strength, Yield | 310 MPa | 45000 psi | Annealed |
California Fine Wire Copper Clad 1006 Steel (40% Conductivity) All values may vary dependent on specific design and usage1006 steel core, 99.99% copper cladCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
Annealed |
AK Steel 309S Austenitic Stainless steel AK Steel 309S provides excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. The alloy is non-magnetic as annealed and becomes slightly magnetic w.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
|
Carpenter 20Cb-3® Stainless Steel Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
|
AK Steel 430 Ferritic Stainless steel AK Steel 430 combines good corrosion resistance and heat and oxidation resistance up to 1500°F with good mechanical properties. Typical consumer applications include automotive trim and molding, f.. |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
AK Steel ASTM A 607 Class 1 Formable, Grade 45K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec.. |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, High Strength Low Alloy Steel (HSLA), 055XLK SAE Specified properties not covered by ASTMInformation provided by AK Steel |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
Annealed |
ATI Allegheny Ludlum 420 Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Tensile Strength, Yield | 310 MPa | 45000 psi | Typical |
ATI Allegheny Ludlum AL 400™ Nickel-Base Alloy, Hot Rolled Plate, UNS N04400 Moderately to faintly magnetic at room temperature. Allegheny Ludlum AL 400 alloy is a ductile nickel-copper alloy with resistance to a variety of corrosive conditions. The alloy is most frequentl.. |
|||
Tensile Strength, Yield | 310 MPa | 45000 psi | Typical |
ATI Allegheny Ludlum Type AL 441HP™ Stainless Steel Alloy Allegheny Ludlum stainless Type AL 441HP™ alloy is a heat resisting ferritic grade providing good oxidation and corrosion resistance for applications like automotive exhaust system components. Dua.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 %, Temperature 93.0 °C |
45000 psi @Strain 0.200 %, Temperature 199 °F |
|
Carpenter Gall-Tough® Stainless Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 1.. |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
AK Steel ASTM A 1011, Class 1 Formable, Grade 45K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
AK Steel ASTM A 570, Grade 45 Hot Rolled Carbon Steel, Structural Quality (SQ) For gauges up to 0.229", ASTM A 570 must be specified, gauges >0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information p.. |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
AK Steel CL 2/ SAE J1392 045 XLK, Grade 45 Cold Rolled Carbon Steel, High Strength Low Alloy Steel (HSLAS) Information provided by AK Steel |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
|
AK Steel 410 Martensitic Stainless steel AK Steel 410 provides good corrosion resistance plus high strength and hardness. It is magnetic in both annealed and hardened conditions. A wide range of properties can be developed with different.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420HC Allegheny Ludlum Type 420HC is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainl.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
|
Haynes Hastelloy® G-30® alloy, 31.8 mm thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |