Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 310 MPa | 45000 psi | |
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-216-P Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP.. |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
MetalTek C86200 Med. Tensile Manganese Bronze High strength and hardness copper-zinc alloy.Applications: Steel mill nuts, ordnance parts, worm gears.Information provided by MetalTekCast UNS C86200; Cast Grade C86200; Cast ASTM B271, B584, B148;.. |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
MetalTek MTEK CX-2MW Cast UNS N26022 Severe Corrosion and Heat Resistant Alloy Information provided by MetalTek |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
MetalTek MTEK N155 UNS R30155 Severe Corrosion and Heat Resistant Alloy Information provided by MetalTek |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 %, Temperature 204 °C |
45000 psi @Strain 0.200 %, Temperature 399 °F |
|
Haynes Ultimet® alloy, 1.6 mm sheet Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 %, Temperature 427 °C |
45000 psi @Strain 0.200 %, Temperature 801 °F |
|
Haynes Ultimet® alloy, 6.3-38.1 mm plate Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 310 MPa | 45000 psi | |
Mueller Alloy 3600 Free Cutting Brass (UNS C36000) Machinability: Recently amended and revised to reflect a lower maximum lead percentage; C36000 remains the industry standard for general machining and high volume production. The excellent machinabi.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 %, Temperature 648 °C |
45000 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes 556® alloy, all-weld metal GTAW Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 %, Temperature 93.0 °C |
45000 psi @Strain 0.200 %, Temperature 199 °F |
|
Haynes Hastelloy® C-22® alloy, 12.7-50.8 mm thick bar, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
|
Haynes Hastelloy® G-30® alloy, 9.5 mm thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Yield | 310 MPa | 45000 psi | Annealed |
Special Metals INCONEL® Alloy 600 A nickel-chromium alloy with good oxidation resistance at high temperatures and resistance to chloride-ion stress-corrosion cracking, corrosion by high-purity water, and caustic corrosion. Used for.. |
|||
Tensile Strength, Yield | 310 - 379 MPa | 45000 - 55000 psi | 0.2% offset |
Eagle Brass 210 Gilding Metal, 3/4 Hard CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
Annealed |
AK Steel 309S Austenitic Stainless steel AK Steel 309S provides excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. The alloy is non-magnetic as annealed and becomes slightly magnetic w.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
|
Carpenter 20Cb-3® Stainless Steel Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
|
Carpenter 20-Mo6® Stainless Steel, Plate Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, .. |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
AK Steel ASTM A 1011, Class 2 Formable, Grade 45K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
AK Steel ASTM A 1011, Grade 45 Type 1 Hot Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
AK Steel CL 1/ SAE J1392 045 XLK, Grade 45 Cold Rolled Carbon Steel, High Strength Low Alloy Steel (HSLAS) Information provided by AK Steel |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
Annealed |
ATI Allegheny Ludlum 420 Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Tensile Strength, Yield | 310 MPa | 45000 psi | Typical |
ATI Allegheny Ludlum AL 400™ Nickel-Base Alloy, Hot Rolled Plate, UNS N04400 Moderately to faintly magnetic at room temperature. Allegheny Ludlum AL 400 alloy is a ductile nickel-copper alloy with resistance to a variety of corrosive conditions. The alloy is most frequentl.. |
|||
Tensile Strength, Yield | 310 MPa | 45000 psi | Typical |
ATI Allegheny Ludlum Type AL 441HP™ Stainless Steel Alloy Allegheny Ludlum stainless Type AL 441HP™ alloy is a heat resisting ferritic grade providing good oxidation and corrosion resistance for applications like automotive exhaust system components. Dua.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
|
ATI Allvac® Allcorr® UNS N06110 Nickel Superalloy Uses: Equipment for deep sour gas wells, flue gas desulfurization, chemical and hydrocarbon processing, and pulp and paper.Property values are for samples in the metallurgical condition: 2050°F ann.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® 23 UNS N08020 Specialty Steel Uses: Pressure vessels, pumps, valves, HX tubing and piping for the CPI and HPI. Trays, flanges, fasteners, wire, screens.Property values are for samples in the metallurgical condition: 1700°F anne.. |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
Annealed |
AK Steel 309 Austenitic Stainless steel AK Steel 309 provides excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. The alloy is non-magnetic as annealed and becomes slightly magnetic wh.. |
|||
Tensile Strength, Yield | >= 310 MPa | >= 45000 psi | |
AK Steel CL 2/ SAE J1392 045 XLK, Grade 45 Cold Rolled Carbon Steel, High Strength Low Alloy Steel (HSLAS) Information provided by AK Steel |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
|
AK Steel 435 Mod Ferritic Stainless steel Information provided by AK Steel |
|||
Tensile Strength, Yield | 310 MPa @Strain 0.200 % |
45000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420HC Allegheny Ludlum Type 420HC is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainl.. |