Tensile Strength, Yield 130 - 265 MPa
18900 - 38400 psi
Average value: 212 MPa Grade Count:54
Overview of materials for Nylon 66, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
Tensile Strength, Yield 131 - 265 MPa

@Temperature -20.0 - 93.3 °C
19000 - 38400 psi

@Temperature -4.00 - 200 °F
Average value: 179 MPa Grade Count:2
Overview of materials for Nylon 66, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..