Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Engineered Polymers DEXFLEX® 711-300 TPO  (discontinued **)

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO) , Polyolefin
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Engineered Polymers DEXFLEX® 711-300 TPO  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: DEXFLEX® 711-300 is a thermoplastic olefinic elastomer compound with post-industrial/post-consumer recycled materials. It is designed for use in applications that are (non-color matched) black, and that require very good processing characteristics. Applications: Wheel liners, filler panels, fan shrouds, air dams, and sight shields Information provided by Solvay Engineering PolymersLyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Linear Mold Shrinkage 0.0090 - 0.011 cm/cm
0.0090 - 0.011 in/in
ASTM D995
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.3 MPa
2510 psi
2 in/min, Type 1; ASTM D638
Flexural Modulus 1.52 GPa
220 ksi
0.05 in/min, 1x3"; ASTM D790
Thermal Properties Metric English Comments
CTE, linear 71.0 µm/m-°C

@Temperature 20.0 °C
39.4 µin/in-°F

@Temperature 68.0 °F
modified; ASTM D696