Mechanical Properties Metric English Comments
Tensile Strength, Yield 1.70 - 44.1 MPa
247 - 6400 psi
Average value: 11.3 MPa Grade Count:147
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a..