Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 82.7 - 155 MPa | 12000 - 22500 psi | Average value: 119 MPa Grade Count:81 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Tensile Strength, Yield | 64.0 - 155 MPa | 9280 - 22500 psi | Average value: 100 MPa Grade Count:6 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Tensile Strength, Yield | 35.0 - 155 MPa | 5080 - 22500 psi | Average value: 58.5 MPa Grade Count:161 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |