PSM Industries Pacific Sintered Metals Infiltrated Iron FX-226-T Powdered Metal

Category Metal , Ferrous Metal
Manufacturer PSM Industries
Trade Name Pacific Sintered Metals
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PSM Industries Pacific Sintered Metals Infiltrated Iron FX-226-T Powdered Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Machines and plates well, Good in hydraulic applications, Moderate tolerance control Equivalent MPIF Specifications: FX-1000-25Information Provided by Pacific Sintered Metals, a division of PSM Industries
Physical Properties Metric English Comments
Density 7.20 - 7.50 g/cc
0.260 - 0.271 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 65
65
Tensile Strength, Ultimate 352 MPa
51000 psi
Tensile Strength, Yield 221 MPa
32000 psi
Elongation at Break 7.0 %
7.0 %
1 in. gauge
Tensile Modulus 110 GPa
16000 ksi
Flexural Strength 910 MPa
132000 psi
Transverse Rupture
Charpy Impact, Unnotched 33.9 J
25.0 ft-lb