Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1140 - 1240 MPa @Strain 0.200 % |
165000 - 180000 psi @Strain 0.200 % |
|
Materion BrushCAST® 275CT Fine Grain Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Tensile Strength, Yield | 1140 - 1240 MPa @Strain 0.200 % |
165000 - 180000 psi @Strain 0.200 % |
|
Materion BrushCAST® 275C High Strength Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Tensile Strength, Yield | 689 - 1240 MPa | 100000 - 180000 psi | depending on condition of material after heat treatment |
Universal Wire Works 17-4 (AMS 5825) Filler Metal Universal 630 (17Cr-4Ni) is a martensitic precipitation - age hardening stainless steel alloy. Alloy 630 can be welded with all welding processes without preheat; however, to obtain weld metal prope.. |