Universal 630 (17Cr-4Ni) is a martensitic precipitation - age hardening stainless steel alloy. Alloy 630 can be welded with all welding processes without preheat; however, to obtain weld metal properties comparable to those of the parent metal a suitable postweld heat treatment is required.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 689 - 1240 MPa
100000 - 180000 psi
depending on condition of material after heat treatment
Component Elements Properties Metric English Comments
Carbon, C <= 0.050 %
<= 0.050 %
Chromium, Cr 16.5 %
16.5 %
Copper, Cu 3.6 %
3.6 %
Iron, Fe >= 73.3 %
>= 73.3 %
As Remainder
Manganese, Mn <= 0.75 %
<= 0.75 %
Nb + Ta 0.22 %
0.22 %
Nickel, Ni 4.8 %
4.8 %
Phosphorous, P <= 0.025 %
<= 0.025 %
Silicon, Si <= 0.75 %
<= 0.75 %
Sulfur, S <= 0.025 %
<= 0.025 %