Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow DOWLEX™ 2244A Linear Low Density Polyethylene, Cast Film Grade

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer Dow Chemical
Trade Name DOWLEX™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow DOWLEX™ 2244A Linear Low Density Polyethylene, Cast Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOWLEX® 2244A Polyethylene resin is a cast film polymer having superior optics in packaging applications. This material complies with U.S. FDA Regulation 21 CFR 177.1520 c 3.2 (a) food packaging applications. The regulation should be consulted for complete details.Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.916 g/cc
0.0331 lb/in³
Melt Flow 3.3 g/10 min

@Load 2.16 kg
3.3 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 7.6.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 20.0 MPa
2900 psi
Molded property
Film Tensile Strength at Yield, MD 7.60 MPa
1100 psi
Film Tensile Strength at Yield, TD 6.90 MPa
1000 psi
Tensile Strength, Yield 9.70 MPa
1410 psi
Molded property
Elongation at Break 900 %
900 %
Film Tensile Strength at Break, MD 54.5 MPa
7900 psi
Thermal Properties Metric English Comments
Vicat Softening Point 94.0 °C
201 °F
Processing Properties Metric English Comments
Processing Temperature 209 °C
408 °F
Film extrusion temperature
Copyright © lookpolymers.com All Rights Reserved