Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers TufFill NH™ GTPO8290-36 TPO

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer S&E Specialty Polymers
Trade Name TufFill NH™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufFill NH™ GTPO8290-36 TPO.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: A 105°C rated, Flexible, TPO based, Zero Halogen compound, exhibiting excellent processing characteristics with superior physical and low temperature propertiesInformation provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 92.0
92.0
ASTM D2240
Tensile Strength, Yield 13.8 MPa
2000 psi
ASTM D638
12.4 MPa

@Treatment Temp. 136 °C,
Time 605000 sec
1800 psi

@Treatment Temp. 277 °F,
Time 168 hour
Aging
Elongation at Break 210 %
210 %
ASTM D638
178.5 %

@Treatment Temp. 136 °C,
Time 605000 sec
178.5 %

@Treatment Temp. 277 °F,
Time 168 hour
Aging
Thermal Properties Metric English Comments
Brittleness Temperature -55.0 °C
-67.0 °F
ASTM D746
Oxygen Index >= 36.0 %
>= 36.0 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 4.30e+15 ohm-cm
4.30e+15 ohm-cm
ASTM D257
Users viewing this material also viewed the following: