Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil LL 6202.19 Injection Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer Exxon Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LL 6202.19 Injection Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LL 6202 is a narrow molecular weight butane copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that require outstanding tear resistance and low warpage.Availability: Latin America, North America and South America Applications: CapsClosuresLids Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.926 g/cc
0.0335 lb/in³
ASTM D4883
Environmental Stress Crack Resistance 180 hour
180 hour
Condition B, 10%; ASTM D1693
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 190 °C
12 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 12.4 MPa
1800 psi
ASTM D638
Elongation at Break 750 %
750 %
ASTM D638
Flexural Modulus 0.407 GPa
59.0 ksi
2% secant; ASTM D790
Flexural Modulus, 1% Secant 455 MPa
66000 psi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 123 °C
253 °F
ASTM D3418
Vicat Softening Point 96.7 °C
206 °F
ASTM D1525
Descriptive Properties Value Comments
Features Standard processing antioxidants
Form PELLET
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved