Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 586 - 703 MPa | 85000 - 102000 psi | 0.2% offset |
Eagle Brass 510 Phosphor Bronzes 5% A, Extra Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Tensile Strength, Yield | 607 - 703 MPa | 88000 - 102000 psi | 0.2% offset |
Eagle Brass 725 Copper Nickel Tin, Extra Spring Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Tensile Strength, Yield | 590 - 700 MPa @Strain 0.200 % |
85600 - 102000 psi @Strain 0.200 % |
|
CLAL-MSX SICLANIC S® TH4 Quenched Copper Alloy, 4/4 Hard, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Tensile Strength, Yield | 600 - 700 MPa | 87000 - 102000 psi | |
ArcelorMittal Complex Phase Steel 800 Y600 Very high strength steel, Cold Rolled Steel Available in the following: uncoated (HCT780C), electrogalvanized (HCT780C+ZE) and Extragal®/Galvannealed (HCT780+Z)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS .. |