Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 586 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 586 MPa

@Temperature 21.1 °C
85000 psi

@Temperature 70.0 °F
0° Direction, Dry; ASTM D638
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 3K 8HS Carbon Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Tensile Strength, Yield 586 MPa

@Temperature 23.9 °C
85000 psi

@Temperature 75.0 °F
0° Direction, Dry; ASTM D638
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 581 Quartz Reinforced
Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low ..
Tensile Strength, Yield 586 MPa
85000 psi
Typical
Kinetics MIM F1537 (ASTM F1537) HIP and Heat Treat
Most commonly used within the medical market on applications requiring these characteristics: Bio-compatibility Corrosion resistance High strength Nonmagnetic Wear resistance. Information prov..
Tensile Strength, Yield >= 586 MPa

@Diameter 3.17 - 88.9 mm,
Strain 0.200 %
>= 85000 psi

@Diameter 0.125 - 3.50 in,
Strain 0.200 %
mid-radius; ASTM E-8
H.C. Starck Molybdenum Hafnium Carbide Powder, Metallurgy Alloy Bar MHC
Description of Product: This specification covers molybdenum alloy (molybdenum + 1.2% hafnium) wrought bar produced from pressed and sintered metallurgy billet.Structure: The MHC alloy bars can be..
Tensile Strength, Yield 586 MPa

@Strain 0.200 %
85000 psi

@Strain 0.200 %
Haynes Ultimet® alloy, aged 1000 hours at 649°C (1200°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Tensile Strength, Yield 586 MPa

@Strain 0.200 %
85000 psi

@Strain 0.200 %
Haynes Ultimet® alloy, all-weld metal, GMAW weld (spray)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Tensile Strength, Yield 586 MPa

@Strain 0.200 %
85000 psi

@Strain 0.200 %
Haynes Hastelloy® C-22® alloy, GTAW, aged 4000 hours at 450°C (800°F), notched
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Tensile Strength, Yield 586 - 703 MPa
85000 - 102000 psi
0.2% offset
Eagle Brass 510 Phosphor Bronzes 5% A, Extra Hard
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
Tensile Strength, Yield >= 586 MPa
>= 85000 psi
0.2% offset
Eagle Brass 7026 Copper Nickel, 1/2 Hard
7026 is a high performance alloy used in springs, terminals, elevated temperature interconnects and high reliability telecommunication components.Information provided by Eagle Brass Company
Tensile Strength, Yield >= 586 MPa
>= 85000 psi
0.2% offset
Eagle Brass 70265 XP175, 1/2 Hard
Information provided by Eagle Brass Company
Tensile Strength, Yield 586 MPa
85000 psi
CMW® 2000 AMS-T-21014 ASTM B777 High Density Machinable Tungsten
Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc.
Tensile Strength, Yield 586 MPa
85000 psi
Typical
Dura-Bar 100-70-03 Continuously Cast Ductile Iron Bar Stock ASTM A536
Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for..
Tensile Strength, Yield 586 MPa

@Strain 0.200 %
85000 psi

@Strain 0.200 %
ATI Allegheny Ludlum AL 4466™ Ferritic Stainless Steel
Low carbon, low nitrogen ferritic stainless steel alloy. Characteristics:outstanding resistance to chloride pitting and crevice corrosion, improved resistance over austenitic stainless steels to ch..
Tensile Strength, Yield 586 MPa

@Strain 0.200 %
85000 psi

@Strain 0.200 %
ATI Allvac® 3-2.5 Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal
Data provided by Allvac.Applications: Excellent cold formability, 20-50% higher tensile properties than CP titanium grades. Primarily used in aircraft hydraulic systems.
Tensile Strength, Yield 586 MPa
85000 psi
HP Alloys Alloy 718, 5% Cold Worked
5% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internatio..
Tensile Strength, Yield 586 MPa

@Strain 0.200 %,
Temperature -73.0 °C
85000 psi

@Strain 0.200 %,
Temperature -99.4 °F
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 10% Cold Work
Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®..
Tensile Strength, Yield 586 - 669 MPa
85000 - 97000 psi
0.2% offset
Eagle Brass 752 Nickel Silver 18%, Extra Hard
Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info..
Copyright © lookpolymers.com All Rights Reserved