Polymer Property : Tensile Strength, Yield = 590 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 590 MPa

@Strain 0.200 %
85600 psi

@Strain 0.200 %
Hogen HM3000 Tungsten-Based Metal
Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; AMS T-21014 Class 3. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a l..
Tensile Strength, Yield 590 MPa

@Strain 0.200 %
85600 psi

@Strain 0.200 %
Hogen HM3750 Tungsten-Based Metal
Mil Spec T-21014D Class 4; ASTM B-777-99 Class 4; AMS T-21014 Class 4. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE..
Tensile Strength, Yield 590 MPa

@Strain 0.200 %
85600 psi

@Strain 0.200 %
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 11.1 mm thick plate
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Tensile Strength, Yield 590 MPa

@Strain 0.200 %
85600 psi

@Strain 0.200 %
Mi-Tech Metals HD18 Tungsten-Based Metal
Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; ASTM B-777-07 Class 3; AMS T-21014 Class 3. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offers high therm..
Tensile Strength, Yield 590 MPa

@Strain 0.200 %
85600 psi

@Strain 0.200 %
Mi-Tech Metals HD18.5 Tungsten-Based Metal
Mil Spec T-21014D Class 4; ASTM B-777-99 Class 4; ASTM B-777-07 Class 4; AMS T-21014 Class 4. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal con..
Tensile Strength, Yield >= 590 MPa
>= 85600 psi
SSAB Tunnplat Domex® 590XP Extra High-strength Cold-forming Steel
Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene..
Tensile Strength, Yield 590 - 700 MPa

@Strain 0.200 %
85600 - 102000 psi

@Strain 0.200 %
CLAL-MSX SICLANIC S® TH4 Quenched Copper Alloy, 4/4 Hard, precipitation treated
SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver..