Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 27.6 MPa
4000 psi
ASTM D882
Westlake EF444 4.7% Ethylene Vinyl Acetate Copolymer  (discontinued **)
Excellent haze and gloss, excellent impact strength and very good sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, section 177..
Film Tensile Strength at Break, MD 27.6 MPa
4000 psi
ASTM D882
LyondellBasell Petrothene® NA345009 Low Density Polyethylene (Film Extrusion)
ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil..
Film Tensile Strength at Break, MD 27.6 MPa
4000 psi
ASTM D882
LyondellBasell Petrothene® NA345013 Low Density Polyethylene (Film Extrusion)
ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil..
Film Tensile Strength at Break, MD 27.6 MPa
4000 psi
ASTM D882
LyondellBasell Petrothene® NA345184 Low Density Polyethylene (Film Extrusion)
ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil..
Film Tensile Strength at Break, MD 27.6 MPa
4000 psi
ASTM D882
LyondellBasell Petrothene® NA345196 Low Density Polyethylene (Film Extrusion)
ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil..
Film Tensile Strength at Break, MD 27.6 MPa
4000 psi
ASTM D882
LyondellBasell Petrothene® NA443023 Blown Low Density Polyethylene
ApplicationsPETROTHENE NA 443 is a series of low density/EVA copolymer resins for high impact/high clarity packaging applications. NA 443 exhibits excellent processability and good balance of optic..
Film Tensile Strength at Break, MD 27.6 MPa
4000 psi
ASTM-D882
Westlake EB502 12.5% EVA Copolymer
Westlake Elevate™ EB502 resin is a fractional melt index 12.5% VA ethylene vinyl acetate copolymer designed for flexible packaging and other films that require excellent toughness and good heat sea..
Film Tensile Strength at Break, MD 27.6 MPa
4000 psi
ASTM D882
Westlake Elevate™ EF439 4.0% Ethylene Vinyl Acetate Copolymer
Excellent haze and gloss, excellent impact strength and very good heat sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, sectio..
Film Tensile Strength at Break, MD 27.6 MPa
4000 psi
ASTM D638
Westlake Elevate™ EF598 9% Ethylene Vinyl Acetate Copolymer
Westlake EF437 resin is a 2.5% EVA copolymer designed for films that require excellent optical and strength properties. This Kosher compliant resin has excellent heat sealing characteristics and low..
Film Tensile Strength at Break, MD 27.6 MPa
4000 psi
ASTM D638
Westlake EMAC® EF598AA 9% Ethylene-Methyl Acrylate Copolymer
Clarity optics, excellent drawdown, excellent machinability, good TD heat shrinkage and excellent toughness. Uses include food packaging tie layers, heat seal layers, extrusion coating, cast film, ..
Film Tensile Strength at Break, MD 27.6 MPa
4000 psi
ASTM D882
Westlake LF1040 Butene Linear Low Density Polyethylene
Westlake LF1040 is a butene LLDPE resin with excellent mechanical and sealing properties. It can be used in stretch film and can liner applications, and is suitable for blending with LDPE in packagi..
Film Tensile Strength at Break, MD 27.6 MPa
4000 psi
Non-oriented film; ASTM D882
Total PPR 7450HC Polypropylene, Film Extrusion Grade
Random copolymer heat sealable film gradeColor - Low catalyst residuals in FINA 7450HC result in improved color stability.Clarity/Impact - The random copolymer structure of FINA 7450HC improves its ..
Film Tensile Strength at Break, MD 27.6 MPa
4000 psi
Dow LDPE 682I Low Density Polyethylene, Film Grade
DOW LDPE 682I barefoot resin is used for shrink, frozen food, and heavy duty film applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact applications. T..
Film Tensile Strength at Break, MD 27.6 MPa
4000 psi
Dow LDPE 683I Low Density Polyethylene, Film Grade
DOW LDPE 683I resin is a general purpose resin with low levels of antiblock additive used for frozen food, and heavy duty film applications. This material complies with U.S.FDA regulation 21 CFR 177..