Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Petrothene® NA443023 Blown Low Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® NA443023 Blown Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPETROTHENE NA 443 is a series of low density/EVA copolymer resins for high impact/high clarity packaging applications. NA 443 exhibits excellent processability and good balance of optics and strong heat sealing characteristics. Regulatory StatusNA 443 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1350. This regulation allows the use of this ethylene vinyl acetate copolymer "…in articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesNA 443 has excellent drawdown characteristics that yield outstanding output rates. Optimum properties are obtained over a broad range of extrusion conditions at melt temperatures between 330°-380°F melt temperatures and a blow-up ratio between 1.7-3.0:1. Using proper techniques and equipment, NA 443 can be drawn to 1.0 mil at commercial production rates. Specific recommendations for the processing of NA 442 can be made only when the end use application, required properties and the processing equipment are known. For exact recommendations, please contact your Equistar representative.Physical PropertiesThese are typical values and not to be construed as specific product limits. Data obtained from film produced in a 3.5"(89mm) blown film line, commercially available 8"(203 mm)die, 375°F(191°C) melt extrusion temperature, 2:1 BUR, 1.25 mil (32 micron) gauge, 0.025"die gap at 130 lb/hr.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.927 g/cc
0.0335 lb/in³
ASTM D1501
Vinyl Acetate Content 4.5 %
4.5 %
Thickness 31.8 microns
1.25 mil
2:1 BUR; 25 mil die gap
Melt Flow 1.2 g/10 min
1.2 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 350 %
350 %
ASTM D882
Film Elongation at Break, TD 550 %
550 %
ASTM D882
Elmendorf Tear Strength MD 140 g
140 g
ASTM D1922
Dart Drop Test 150 g
0.331 lb
F<sub>50</sub>; ASTM D1709
Film Tensile Strength at Break, MD 27.6 MPa
4000 psi
ASTM D882
Film Tensile Strength at Break, TD 20.0 MPa
2900 psi
ASTM D882
1% Secant Modulus, MD 138 MPa
20000 psi
ASTM D882
1% Secant Modulus, TD 124 MPa
18000 psi
ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 88.0 °C
190 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 3.0 %
3.0 %
ASTM D1003
Gloss 77 %
77 %
at 45°; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 191 °C
375 °F
Descriptive Properties Value Comments
Antiblock None
Slip None
Users viewing this material also viewed the following: