Material Notes:
Clarity optics, excellent drawdown, excellent machinability, good TD heat shrinkage and excellent toughness. Uses include food packaging tie layers, heat seal layers, extrusion coating, cast film, and compounding.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.931 g/cc
0.0336 lb/in³
ASTM D1505
Methyl Acrylate Content 9.0 %
9.0 %
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Dart Drop 4.45 g/micron
113 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 27.6 MPa
4000 psi
ASTM D638
Film Tensile Strength at Break, TD 20.7 MPa
3000 psi
ASTM D638
1% Secant Modulus, MD 89.6 MPa
13000 psi
ASTM D882
1% Secant Modulus, TD 110 MPa
16000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 97.0 °C
207 °F
Peak; ASTM D3418
Optical Properties Metric English Comments
Haze 4.8 %
4.8 %
ASTM D1003
Descriptive Properties Value Comments
Process Extrusion
Film