Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 310 g | 310 g | ASTM D1922 |
ExxonMobil LD 135.09 Blown Film Resin
(discontinued **) LD 135.09 is a homopolymer film resin with good clarity. Applications include food packaging, light to medium duty bags, and textile packaging.Information provided by ExxonMobil Chemical |
|||
Elmendorf Tear Strength MD | 310 g | 310 g | ASTM D1922 |
ExxonMobil LD 144.50 Packaging Film Resin Film made from LD 144.50 offers improved impact strength and heat sealability compared to homopolymer clarity film resins. Typically applications include food packaging, frozen food packaging, and .. |
|||
Elmendorf Tear Strength MD | 310 g | 310 g | ASTM-D1922 |
Braskem LBH0120PBS LLDPE Blown Film Extrusion Polyethylene Copolymer LBH0120BPS is a LLDPE Hexene copolymer produced by Braskem. It is a general purpose product that shows a good processing performance balanced with good optical and mechanical properties as well as s.. |
|||
Elmendorf Tear Strength MD | 310 g | 310 g | ASTM-D1922 |
Braskem TN7006 LDPE Blown Film Extrusion Polyethylene TN7006 is a low-density polyethylene (LDPE) specially developed for coextruded films and lamination. The resin presents a great combination of mechanical, optical, and stiffness properties. TN7006 h.. |
|||
Elmendorf Tear Strength MD | 310 g | 310 g | ASTM-D1922 |
Braskem TS7006 LDPE Blown Film Extrusion Polyethylene TS7006 is a low-density polyethylene (LDPE) specially developed for coextruded films and lamination. The resin presents a combination of mechanical, optical, and stiffness properties. TS7006 has a l.. |
|||
Elmendorf Tear Strength MD | 310 g | 310 g | ASTM-D1922 |
Braskem TS7010 LDPE Blown Film Extrusion Polyethylene TS7010 is a low-density polyethylene (LDPE) that presents excellent processability and good mechanical properties. The incorporated additives package warrants a low coefficient of friction (COF) all.. |