Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 37.9 - 51.0 MPa | 5500 - 7400 psi | ASTM D882 |
Honeywell Capran® K Coated Nylon Film
(discontinued **) Description: Capran® K is a PVdc coated nylon 6 film designed for food packaging applications where longer shelf life is required. This film exhibits good clarity, gloss, toughness, thermoformabil.. |
|||
Film Tensile Strength at Yield, MD | 37.9 - 51.0 MPa | 5500 - 7400 psi | ASTM D882 |
Honeywell Capran® Nylon Film, Multipurpose Nylon 6 Film Description: Capran® is a multipurpose nylon 6 film. Its physical properties are evenly distributed for optimum performance giving excellent resistance to flex cracking. It can be processed ove.. |
|||
Film Tensile Strength at Yield, MD | 37.9 MPa | 5500 psi | ASTM D882 |
ExxonMobil HDPE HD 7960..13 High Density Polyethylene Resin Product Description: HD 7960.13 is a high molecular weight HDPE blown film resin. Films made from HD 7960.13 exhibit excellent impact and toughness properties, as well as high stiffness. HD 7960.13 .. |
|||
Film Tensile Strength at Yield, MD | 37.9 MPa | 5500 psi | ASTM D882 |
ExxonMobil HD 7960.13 HMW Blown Film Resin Product Description: HD 7960.13 is a high molecular weight HDPE blown film resin. Films made from HD 7960.13 exhibit excellent impact and toughness properties, as well as high stiffness. HD 7960.13 .. |