Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.210 MPa-m/sec
6000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Ertalyte® TX Internally Lubricated Semi-Crystalline Polyester (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.210 MPa-m/sec
6000 psi-ft/min
at 1 m/s unlubricated
Quadrant EPP Ketron® 1000 PEEK unfilled, extruded (ISO Data)
Ketron PEEK-1000 stock shapes are produced from virgin polyetheretherketone resin and offer the highest toughness and impact strength of all Ketron PEEK grades. Both Ketron PEEK-1000 natural & black..
Limiting Pressure Velocity 0.210 MPa-m/sec
6000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Nylatron® LFG (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.210 MPa-m/sec
6000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Nylatron® LIG Oil Filled Cast 6 Nylon (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.210 MPa-m/sec
6000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Semitron® MPR-1000 (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.210 MPa-m/sec
6000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP TIVAR® HPV UHMW-PE (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.210 - 1.26 MPa-m/sec
6000 - 36000 psi-ft/min
Average value: 0.509 MPa-m/sec Grade Count:11
Overview of materials for Polyetheretherketone, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value..
Limiting Pressure Velocity 0.210 MPa-m/sec
6000 psi-ft/min
4:1 safety factor applied; QTM 55010
Quadrant EPP Semitron® CMP LL5 Polyester (ASTM Product Data Sheet)
Enhanced semi-crystalline polyester product for extended service in CMP retaining rings. Superior performance, especially in oxide processes, and cost effective relative to standard ring materials. ..
Limiting Pressure Velocity 0.210 MPa-m/sec
6000 psi-ft/min
LNP EPALP-TB003, at 100 ft/min
Ensinger HYDEX® 4101 Polybutylene Terephthalate (PBT)
HYDEX® 4101 & 4101L (lubricated) is a very stable chemical compound that can withstand high impact without deterioration. It is approved for direct contact with food by the FDA and is ideal for ma..
Limiting Pressure Velocity 0.210 MPa-m/sec
6000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Semitron® ESd 500 HR PTFE, static dissipative, compression molded (ASTM Product Data Sheet)