Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.210 - 1.26 MPa-m/sec | 6000 - 36000 psi-ft/min | Average value: 0.509 MPa-m/sec Grade Count:11 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |