Quadrant EPP Ketron® HPV PEEK High Pressure Velocity Polyetherether Ketone (ASTM Product Data Sheet)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Quadrant Engineering Plastics Products
Trade Name Ketron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Ketron® HPV PEEK High Pressure Velocity Polyetherether Ketone (ASTM Product Data Sheet).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This bearing grade of extruded Ketron PEEK offers the lowest coefficient of friction and best machinability of all Ketron grades. It is ideal for low wear, high PV parts that require chemical resistance.Data provided by Quadrant Engineering Plastic Products. Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to hot water or steam
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc

@Temperature 22.8 °C
1.44 g/cc

@Temperature 73.0 °F
ASTM D792
Water Absorption 0.050 %
0.050 %
Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 0.30 %
0.30 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 85
85
ASTM D785
Tensile Strength 75.8 MPa

@Temperature 22.8 °C
11000 psi

@Temperature 73.0 °F
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Tensile Modulus 5.86 GPa

@Temperature 22.8 °C
850 ksi

@Temperature 73.0 °F
ASTM D638
Flexural Strength 190 MPa

@Temperature 22.8 °C
27500 psi

@Temperature 73.0 °F
ASTM D790
Flexural Modulus 7.58 GPa

@Temperature 22.8 °C
1100 ksi

@Temperature 73.0 °F
ASTM D790
Compressive Strength 138 MPa

@Strain 10.0 %,
Temperature 22.8 °C
20000 psi

@Strain 10.0 %,
Temperature 73.0 °F
ASTM D732
Compressive Modulus 3.45 GPa

@Temperature 22.8 °C
500 ksi

@Temperature 73.0 °F
ASTM D695
Shear Strength 68.9 MPa

@Temperature 22.8 °C
10000 psi

@Temperature 73.0 °F
ASTM D790
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256 Type A
Coefficient of Friction, Dynamic 0.21
0.21
Dry vs. Steel; QTM 55007
K (wear) Factor 201 x 10-8 mm³/N-M
100 x 10-10 in³-min/ft-lb-hr
QTM 55010
Limiting Pressure Velocity 0.701 MPa-m/sec
20000 psi-ft/min
4:1 safety factor; QTM 55007
Thermal Properties Metric English Comments
CTE, linear 30.6 µm/m-°C

@Temperature -40.0 - 149 °C
17.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Thermal Conductivity 0.245 W/m-K
1.70 BTU-in/hr-ft²-°F
ASTM F433
Melting Point 340 °C
644 °F
Crystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 250 °C
482 °F
Long Term
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
383 °F
ASTM D648
Flammability, UL94 V-0
V-0
1/8 inch (Estimated Rating)
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 10000 ohm
<= 10000 ohm
EOS/ESD S11.11
Compliance Properties Metric English Comments
3A-Dairy No
No
Canada AG No
No
FDA No
No
NSF No
No
USDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Limited
Limited
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Acceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Acceptable
Acceptable
Conductive / Static Dissipative Yes
Yes
Continuous Sunlight Acceptable
Acceptable
Hot Water / Steam Acceptable
Acceptable
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable
Descriptive Properties Value Comments
Color Natural
Machinability 7
1-10, 1=Easier to Machine