Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.0701 - 0.590 MPa-m/sec
2000 - 16800 psi-ft/min
Average value: 0.167 MPa-m/sec Grade Count:8
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..