Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.0701 MPa-m/sec | 2000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Armor-X™ Non-Marring, Elastomer Polymeric Blend (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.0701 MPa-m/sec | 2000 psi-ft/min | 4:1 safety factor applied; QTM 55010 |
Quadrant EPP Durapro® Truck Liners (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.0700 MPa-m/sec | 2000 psi-ft/min | at 1 m/s unlubricated |
Quadrant EPP Ertalon® 6 SA PA 6, extruded (ISO Data) This material offers an optimal combination of mechanical strength, stiffness, toughness, mechanical damping properties and wear resistance. These properties, together with good electrical insulatin.. |
|||
Limiting Pressure Velocity | 0.0701 MPa-m/sec | 2000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP TIVAR® Dockguard - UHMW-PE - Black UV Stabilized UHMW-PE (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.0701 MPa-m/sec | 2000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP TIVAR® Extended Wear UHMW-PE, Premium Glass-filled, Partially Cross-linked (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.0701 MPa-m/sec | 2000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP TIVAR® SuperPlus UHMW-PE, Glass-filled Cross-linked & Heat Stabilized Extreme Wear Resistant (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.0701 - 0.590 MPa-m/sec | 2000 - 16800 psi-ft/min | Average value: 0.167 MPa-m/sec Grade Count:8 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Limiting Pressure Velocity | 0.0700 MPa-m/sec | 2000 psi-ft/min | without lubrication; MPC Test |
Manifattura Cattaneo PA 6 Nylon Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Limiting Pressure Velocity | 0.0701 MPa-m/sec | 2000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Quicksilver® UHMW-PE Premium Truck Lining (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.0701 MPa-m/sec | 2000 psi-ft/min | 4:1 safety factor; QTM 55007 |